Pulse deposition of 2.4 T Co37Fe63 alloy in photoresist features with 40 nm critical dimension and high aspect ratio is presented. The design of the pulse deposition parameters is described in terms of the transport limitations through the diffusion layer, electrochemical interface stability with respect to Fe(OH)3 precipitation, and the optimum conditions for additive (Saccharin) adsorption. The alloy grain size and crystal structure in the nanoconfined electrode geometry is compared versus the thin film and relevant implications for magnetic recording are discussed. The 2.4 T Co38Fe61Pd1 alloy is introduced as a possible way to improve the corrosion properties of 2.4 T Co37Fe63 alloy. [ABSTRACT FROM AUTHOR]
- Abstract:
Copyright of IEEE Transactions on Magnetics is the property of IEEE and its content may not be copied or emailed to multiple sites or posted to a listserv without the copyright holder's express written permission. However, users may print, download, or email articles for individual use. This abstract may be abridged. No warranty is given about the accuracy of the copy. Users should refer to the original published version of the material for the full abstract. (Copyright applies to all Abstracts.)
No Comments.